Analysis of Flip-Chip Assembly Technology on Flexible Circuit Boards

The ability to control machines with one's thoughts has long been a human dream, particularly for those with paralysis. In recent years, technological advancements have accelerated progress in Brain-Machine Interfaces (BMIs). For biomedical applications, researchers at Duke University have successfully developed signal-processing ASICs using neural probes, as well as electronic circuit systems for the wireless transmission of power and data. The next step is the development of component packaging technology. However, how will these components be interconnected?
Size and reliability are the two most critical factors for biomedical implants. Two packaging technologies from the microelectronics industry—flip-chip bonding and flexible substrates—are ideally suited for this application. Flip-chip bonding technology has been in development for over 30 years. Its advantages include compact size and high interconnect density; furthermore, electrical performance is improved due to shorter interconnect paths. Another advantage of flip-chip bonding is the ability to mount multiple chips of varying sizes onto a single substrate to form a multi-chip module. This packaging approach eliminates the need for bulky and unreliable connectors.

Additionally, flexible substrates made of polyimide can bend and fold, allowing for efficient space utilization and the creation of compact components. However, since polyimide materials are compatible only with low-temperature bonding techniques (processing temperatures below 200°C), thermosetting adhesives—rather than solder—must be used to establish mechanical and electrical connections. In this study, we employed a low-cost gold pillar bump technology, as opposed to the tin-lead bump technology used in other similar applications.

To develop a process suitable for biomedical applications, we designed and fabricated test chips using polyimide substrates. These chips, featuring gold pillar bumps, were used to validate the manufacturing process. We tested both conductive and insulating thermosetting adhesives and evaluated product reliability by measuring contact resistance following thermal cycling tests. Bonding Technology
We aimed to develop a reliable process for bonding diced chips onto flexible substrates using stud gold bumps and thermosetting adhesive. In this study, we evaluated two bonding methods: the first utilized an insulating thermosetting adhesive, while the second employed a conductive adhesive combined with an insulating underfill. Each test assembly consisted of a circuit substrate and a dummy chip. A substrate layout for a pin-grid array package was also designed on the same polyimide substrate to facilitate future testing of neural signal amplifier chips.

Dummy Chip Preparation: To ensure the flexible dummy chip possessed rigidity comparable to a silicon chip, a stiffener was required on its backside. However, as the stiffener provided by the substrate manufacturer was too soft, we replaced it with a small piece of 1 mm-thick microscope slide glass. Stud Gold Bumps: The stud gold bumps on the dummy chips used in the tests were fabricated using a manual gold ball bonder (Kulicke & Soffa Model 4524AD).
Bonding with Insulating Thermosetting Adhesive: In this method, the chip (featuring stud gold bumps) and the substrate were bonded using an insulating thermosetting adhesive. Alignment and bonding were performed using a flip-chip bonder (SUSS Microtec Model FC150). The bonding procedure was as follows:
1. Load the chip (with stud gold bumps) and the substrate into the flip-chip bonder.
2. Align the chip and the substrate using the flip-chip bonder.
3. Dispense the insulating thermosetting adhesive onto the substrate.
4. Bond the chip to the substrate according to the conditions specified in Table 2 and Figure 3. 5. The adhesive is thermally cured under bonding pressure and then cooled before the pressure is released.

Conductive Adhesive Bonding Technique
In the conductive adhesive bonding method, a chip featuring cylindrical gold bumps is first placed into a thin layer of silver adhesive. The chip, now coated with silver adhesive, is then bonded to the carrier board using an insulating thermosetting adhesive. A flip-chip bonder is used for both the alignment and bonding of the chip to the carrier board. The bonding steps are as follows:
1. Load the chip (with cylindrical gold bumps) onto the flip-chip bonder.
2. Place a glass slide onto the vacuum chuck designed for the carrier board.
3. Apply a thin layer of conductive silver adhesive onto the glass slide. Note: Dilute the conductive silver adhesive by 10% to achieve better adhesion.
4. Use the flip-chip bonder to spread the conductive silver adhesive to a thickness of 30 micrometers.
5. Press the chip (with cylindrical gold bumps) into the 30-micrometer-thick layer of conductive silver adhesive.
6. Remove the glass slide and place the carrier board in position.
7. Apply insulating thermosetting adhesive onto the carrier board.
8. Align the chip with the carrier board and bond them together using the adhesive.
9. The adhesive is thermally cured under bonding pressure and then cooled before the pressure is released.

Temperature Cycling Test: Temperature cycling tests are frequently used to verify the reliability of bonding joints. During the test, the temperature and the resistance between a pair of bumps on the dummy chip are recorded every 30 seconds.
The temperature cycling conditions are set as follows:
1. Hold at 85°C for 10 minutes.
2. Cool down to -10°C at the maximum possible rate.
3. Hold at -10°C for 10 minutes. 4. Heat up to 85°C as rapidly as possible.
5. Repeat this temperature cycling process.

The dummy chips were diced from the polyimide substrate, bonded to glass slides to enhance the structural rigidity of the flexible chips, and fitted with cylindrical gold bumps; they were then bonded to the flexible carrier board using the two previously mentioned methods (bonding with insulating thermosetting adhesive and bonding with conductive thermosetting adhesive). Since the dummy chips fabricated on the polyimide substrate were semi-transparent, we were able to visually inspect the bonding interface. The cylindrical gold bumps appeared to be compressed uniformly, indicating excellent flatness control. Alignment accuracy was maintained within 3 micrometers. While some air bubbles were visible within the adhesive layer, they did not appear to affect performance.

The bonding technique utilizing cylindrical gold bumps and adhesive offers several advantages. First, this method is suitable for singulated (diced) chips. In fact, using flexible dummy chips as test vehicles is a cost-effective and practical approach for developing bonding technologies. The semi-transparency of the test vehicles—an unexpected benefit of using polyimide as the substrate—allowed for easy inspection of bonding quality via optical microscopy. The process using insulating thermosetting adhesive is relatively simple, requiring neither a cleaning step nor additional underfill. Conversely, the conductive adhesive bonding method involves steps that demand precise control, particularly the silver adhesive dispensing and dipping processes; furthermore, an underfill step is required to ensure sufficient mechanical strength. A shared drawback of both methods is the excessively long adhesive curing time (10 minutes); while acceptable for research purposes, a faster-curing adhesive would be necessary for mass production. We believe that the curing of the adhesive and underfill pulls the chip and carrier board tightly together, thereby enhancing the quality of the bond. In thermal cycling tests, the average electrical resistance of assemblies bonded using the insulating thermosetting adhesive technique met our expectations and was comparable to results reported by other groups. Assemblies fabricated by bonding flip-chip ASICs to flexible substrates using this insulating thermosetting adhesive technique demonstrated electrical performance consistent with that of commercially produced ceramic pin-grid array (PGA) packages. Furthermore, this technique offers the advantages of a compact footprint and adaptability to various form factors.
To bond neural signal amplifier ASIC chips onto flexible substrates using flip-chip packaging, we developed and evaluated two bonding methods, utilizing dummy chips fabricated on polyimide substrates for process development and testing. Based on considerations of process simplicity and reliability, we selected the insulating thermosetting adhesive bonding technique combined with cylindrical gold-bump technology. We also applied this method to bond neural signal amplifier ASIC chips onto pin-grid array (PGA) substrates; the initial prototype run yielded a fully functional device.

08 Oct 2026